Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kraton D1192 ETM - SBS - Kraton Polymers

Material Data Center offers the following functions for Kraton D1192 ETM:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kraton D datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Kraton D1192 E is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass.
Kraton D1192 ETM - supplied as powder dusted with talc.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 1 g/10min ISO 1133
温度 200 °C -
荷重 5 kg -
機械的特性単位テスト基準
ISO データ
引張強度 33 MPa ISO 37
破壊ひずみ 1000 % ISO 37
ASTM数据
ショア硬さA 70 - ASTM D 2240
Other Standards[S]
伸び率300%時の応力 14.4 MPa ISO 37
S: These properties are reported by the producer according standards that are different to our defaults.
その他の特性.単位テスト基準
Bulk density 400 kg/m³ -
Other Standards[S]
密度. 940 kg/m³ ISO 2781
S: These properties are reported by the producer according standards that are different to our defaults.
特殊な特性
成形加工法.
コーティング.
納入形状.
パウダー.
特殊な特性.
透明.
な特性
Copolymer
耐薬品性
Oxidation Resistance
領域別の利用可能性
北アメリカ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com